Dielectric Strength 54.29 kV/mm
1379 kV/in
ASTM D149-97a
Lord Adhesives CircuitSAFâ„¢ MA-420 Epoxy Surface Mount Adhesive
CircuitSAFâ„¢ MA-420 is an epoxy surface mount adhesive that cures rapidly at elevated temperatures and has been designed for use in high speed printed circuit board assembly for the attachment o..