Lord Adhesives CircuitSAFâ„¢ MA-420 Epoxy Surface Mount Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Lord Adhesives
Trade Name CircuitSAF™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives CircuitSAFâ„¢ MA-420 Epoxy Surface Mount Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CircuitSAFâ„¢ MA-420 is an epoxy surface mount adhesive that cures rapidly at elevated temperatures and has been designed for use in high speed printed circuit board assembly for the attachment of surface mount components. This product is unique in that it can be used for both high speed dispensing and rapid printing without sacrificing any performance in either application. The high shear thinning and excellent viscosity recovery makes the material an excellent choice for high speed SMT applications. CircuitSAFâ„¢ MA-420 has been successfully used in high speed placement systems with integrated dispense heads. A list of equipment and the corresponding packaging can be found in the CircuitSAFâ„¢ MA-420 Brochure. CircuitSAFâ„¢ MA-420 also shows superior performance in non-contact dispense systems such as the Asymtek Dispense JetTM. The superior dot profile and high dot aspect ratio make it ideal for rapid printing. CircuitSAFâ„¢ MA-420 is fully compatible with the DEK ProFlow DirEKt ImagingTM system and is available in DEK ProFlowTM Cassettes.All information provided by Lord.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
Particle Size <= 50 µm
<= 50 µm
mean particle size, 5 microns
Brookfield Viscosity 100000 cP
100000 cP
2HB CP52 Spindle @ 4.6rpm
2.10e+6 cP
2.10e+6 cP
2HB CP52 Spindle @ 0.1rpm
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.29 GPa
332 ksi
DMTA @ 1kHz
Shear Strength >= 13.8 MPa
>= 2000 psi
IPC817, 5 min 125ºC cure
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C
25.0 µin/in-°F
Alpha 1
140 µm/m-°C
77.8 µin/in-°F
Alpha 2
Thermal Conductivity 0.280 W/m-K
1.94 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg 70.0 °C
158 °F
Flash Point >= 93.0 °C
>= 199 °F
Electrical Properties Metric English Comments
Volume Resistivity 9.00e+15 ohm-cm
9.00e+15 ohm-cm
Insulation Resistance >= 1.00e+9 ohm
>= 1.00e+9 ohm
After 4 days
>= 1.00e+9 ohm
>= 1.00e+9 ohm
After 7 days
Dielectric Constant 3.73

@Frequency 1.00e+9 Hz
3.73

@Frequency 1.00e+9 Hz
ASTM D150-95
3.74

@Frequency 1000 Hz
3.74

@Frequency 1000 Hz
ASTM D2520-95
3.8

@Frequency 10000 Hz
3.8

@Frequency 10000 Hz
ASTM D2520-95
3.9

@Frequency 1.00e+10 Hz
3.9

@Frequency 1.00e+10 Hz
ASTM D2520-95
4.56

@Frequency 1.00e+6 Hz
4.56

@Frequency 1.00e+6 Hz
ASTM D150-95
Dielectric Strength 54.29 kV/mm
1379 kV/in
ASTM D149-97a
Dissipation Factor 0.0083

@Frequency 1000 Hz
0.0083

@Frequency 1000 Hz
ASTM D2520-95
0.0137

@Frequency 10000 Hz
0.0137

@Frequency 10000 Hz
ASTM D2520-95
0.0168

@Frequency 1.00e+9 Hz
0.0168

@Frequency 1.00e+9 Hz
ASTM D150-95
0.031

@Frequency 1.00e+6 Hz
0.031

@Frequency 1.00e+6 Hz
ASTM D150-95
0.0415

@Frequency 1.00e+10 Hz
0.0415

@Frequency 1.00e+10 Hz
ASTM D2520-95
Processing Properties Metric English Comments
Cure Time 1.00 - 1.50 min

@Temperature 150 °C
0.0167 - 0.0250 hour

@Temperature 302 °F
3.00 min

@Temperature 120 °C
0.0500 hour

@Temperature 248 °F
Shelf Life 9.00 Month

@Temperature 0.000 - 25.0 °C
9.00 Month

@Temperature 32.0 - 77.0 °F
Descriptive Properties Value Comments
Appearance Red or Yellow
Electromigration Passed
Bellcore GR-78
Thixotropic Index 12.1
ASTM D2196 (1 and 10rpm)
Torque Strength (N-mm) 68
on 1206 devices