Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.7 - 65.0 kV/mm | 450 - 1650 kV/in | Average value: 32.0 kV/mm Grade Count:19 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Dielectric Strength | 20.0 - 65.0 kV/mm | 508 - 1650 kV/in | DIN 53481 |
Isoflon POM H Polyacetal H Good optical propertiesHigh UV resistanceAbsorbs little moistureInformation provided by Isoflon. |
|||
Dielectric Strength | 20.0 - 65.0 kV/mm | 508 - 1650 kV/in | DIN 53481 |
Isoflon POM C Polyacetal C Good optical propertiesHigh UV resistanceAbsorbs little moistureInformation provided by Isoflon. |