Polymer Property : Dielectric Strength = 688 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 27.1 kV/mm

@Thickness 1.60 mm
688 kV/in

@Thickness 0.0630 in
in oil; ASTM D 149
SABIC Innovative Plastics Geloy XTPM309 ASA+PC (Europe-Africa-Middle East)
XTPM309 is a modified HRA170 with improved processing stability.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Dielectric Strength 27.1 - 38.0 kV/mm
688 - 965 kV/in
Average value: 33.3 kV/mm Grade Count:9
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Dielectric Strength 27.1 kV/mm
688 kV/in
ASTM D149
LyondellBasell Astryn BA35H Polypropylene Copolymer, Flame Retardant
Key Features: conventional melt flow, medium modulus, flame retardant polypropylene copolymer, UL 94 V-2 flames, good electrical properties and insulating characteristics, good aesthetics and colora..
Dielectric Strength 27.1 kV/mm
688 kV/in
ASTM D149
LyondellBasell Astryn BA45H Polypropylene Copolymer, Flame Retardant
Key Features: medium melt flow, medium modulus, flame retardant polypropylene copolymer, UL 94 V-2 flames, good electrical properties and insulating characteristics, good aesthetics and colorability..
Dielectric Strength 27.1 kV/mm
688 kV/in
ASTM D149
LyondellBasell Astryn BA65H Polypropylene Copolymer, Flame Retardant
Key Features: high melt flow, medium modulus, flame retardant polypropylene copolymer, good electrical properties, good aesthetics and colorability, good processabilityApplications: furniture, small..