Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 8.86 - 13.8 kV/mm | 225 - 351 kV/in | Average value: 11.3 kV/mm Grade Count:15 |
Overview of materials for Phenolic; Unreinforced; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Dielectric Strength | 8.86 kV/mm | 225 kV/in | |
GBC L3 Steatite Ideal for high frequency, low loss, high voltage insulation. Much less expensive than alumina insulatorsApplications: resistor forms, surge arrestors, standoffs, spacers, and coil forms.Machinabili.. |
|||
Dielectric Strength | 8.86 kV/mm | 225 kV/in | Step by Step; ASTM D149 |
Sumitomo Bakelite Durez® 32962 Phenolic Molding Compound, Injection Grade Durez 32962 Black Phenolic is a medium impact, molding compound. It is designed for applications where additional mechanical strength is required. Typical applications include appliance housings whe.. |
|||
Dielectric Strength | 8.86 kV/mm | 225 kV/in | |
Aremco AREMCOLOX™ 502-1400 (Full-Fired) Dense Alumina Parts fabricated to print. Excellent physical properties and corrosion resistance. For pump liners, nozzles, guides. Standard crucibles and bolts, nuts and washers from 4-40 to 1/4-20. |