Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 328.1 kV/mm | 8333 kV/in | 100 V/sec |
DuPont Teijin Films Mylar® C Polyester Film, 24 Gauge Mylar® Type C films are available in a wide range of generally thinner gauges (typically 10 through 92) that offer excellent electrical properties, combined with superior strength and dimensional s.. |