Material Notes:
Mylar® Type C films are available in a wide range of generally thinner gauges (typically 10 through 92) that offer excellent electrical properties, combined with superior strength and dimensional stability.Mylar® Type C films offer the ideal combination of tensile strength, dimensional stability, and electrical properties needed for use in capacitors.Mylar® Type C films were developed specifically as a dielectric for use in metallized and film/foil capacitors. Typical capacitor applications include energy storage, frequency discrimination, filtering, coupling, and by-passing.Approvals: UL 94 VTM-2 - for 92 - 500 gauge (0.023 - 0.13mm) and UL Recognition - for 92 - 500 gauge (0.023 - 0.13mm) - HWI=5, HAI=4, CTI=1Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 179 MPa
26000 psi
ASTM D882A
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Shrinkage, MD 2.1 %

@Temperature 150 °C,
Time 1800 sec
2.1 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 150 °C,
Time 1800 sec
1.0 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Refractive Index 1.64 - 1.67
1.64 - 1.67
typical of Mylar®
Electrical Properties Metric English Comments
Dielectric Strength 328.1 kV/mm
8333 kV/in
100 V/sec
Dielectric Breakdown 2000 V
2000 V
100 V/sec
Comparative Tracking Index 400 - 600 V
400 - 600 V
Hot Wire Ignition, HWI <= 7.0 sec
<= 7.0 sec
High Amp Arc Ignition, HAI <= 15 arcs
<= 15 arcs
Descriptive Properties Value Comments
Insulation Resistance 10000 µF