Polymer Property : Dielectric Strength = 838 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 16.0 - 33.0 kV/mm
406 - 838 kV/in
Average value: 23.6 kV/mm Grade Count:3
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and ..
Dielectric Strength 17.7 - 33.0 kV/mm
450 - 838 kV/in
Average value: 26.8 kV/mm Grade Count:5
Overview of materials for Polyamide-Imide, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Dielectric Strength 17.7 - 33.0 kV/mm
450 - 838 kV/in
Average value: 19.8 kV/mm Grade Count:21
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..