Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 9.17 kV/mm | 233 kV/in | ASTM D149 |
Ensinger Tecatron® XP-64 Compression Molded PPS Compound, 40% Fiberglass Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Dielectric Strength | 9.17 kV/mm | 233 kV/in | ASTM D149 |
Ensinger Tecatron® XP-64B Compression Molded PPS Compound, 40% Fiberglass, Black Pigmented Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Dielectric Strength | 9.17 - 30.0 kV/mm | 233 - 762 kV/in | Average value: 19.8 kV/mm Grade Count:49 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |