Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger Tecatron® XP-64 Compression Molded PPS Compound, 40% Fiberglass

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Manufacturer Ensinger
Trade Name Tecatron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecatron® XP-64 Compression Molded PPS Compound, 40% Fiberglass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run production and yields products which are homogenous with low process stress.TECATRON PPS is a highly crystalline high-temperature thermoplastic with an excellent balance of cost, temperature resistance, strength, chemical resistance and flame retardance. TECATRON PPS is often used when long-term high-temperature performance and dimensional stability are a must, even in the presence of aggressive chemicals.Applications:Fuel InjectorsManifoldsPumpsPistonsGearsV-Packing GasketsBearingsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
ASTM D792
Filler Content 40 %
40 %
Water Absorption 0.063 %

@Time 86400 sec
0.063 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
ASTM D2240
Tensile Strength 42.7 MPa
6200 psi
ASTM D638
Elongation at Break 1.1 %
1.1 %
ASTM D638
1.4 %
1.4 %
Flexural Strain; ASTM D790
Tensile Modulus 6.21 GPa
900 ksi
ASTM D638
Flexural Strength 75.8 MPa
11000 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Compressive Strength 172 MPa
25000 psi
ASTM D695
Compressive Modulus 4.00 GPa
580 ksi
ASTM D695
Shear Strength 55.8 MPa
8100 psi
ASTM D732
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 68.4 µm/m-°C
38.0 µin/in-°F
ASTM E831
Electrical Properties Metric English Comments
Volume Resistivity 2.90e+15 ohm-cm
2.90e+15 ohm-cm
ASTM D257
Dielectric Constant 4.6

@Frequency 1.00e+6 Hz
4.6

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 9.17 kV/mm
233 kV/in
ASTM D149
Descriptive Properties Value Comments
Color Dark Brown
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved