Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.0040 ohm-cm | 0.0040 ohm-cm | Chomerics MAT-1002 |
Parker Chomerics CHOFORM® 5513 Conductive Form-in-Place Gasket Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |
|||
Volume Resistivity | 0.0040 ohm-cm | 0.0040 ohm-cm | CEPS-0002 |
Parker Chomerics CHO-SEAL 1291 Conductive Elastomer Commercial Grade Conductive Elastomer. This material is electronically conductive and specially formulated to provide shielding against electromagnetic interference. It is a high-performance Chomeri.. |
|||
Volume Resistivity | <= 0.0040 ohm-cm | <= 0.0040 ohm-cm | |
Parker Chomerics Tecknit Consil®-C 871 Silver-Copper Filled Silicone Elastomer Description: CONSIL-C is a silicone or fluorosilicone elastomer filled with silver-plated copper particles designed to achieve maximum electrical conductivity. CONSIL-C provides one of the highest s.. |
|||
Volume Resistivity | 0.0040 ohm-cm | 0.0040 ohm-cm | CEPS-0002 |
Parker Chomerics CHO-SEAL 1273 Conductive Elastomer Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con.. |
|||
Volume Resistivity | <= 0.0040 ohm-cm | <= 0.0040 ohm-cm | |
Sinotek Materials 2nd Class Carbon Rod for Dry Battery We offer carbon rods for dry batteries in 11 regular sizes, including R03, R1, R6,R10, R12,R14, R20, R25, R40, S4, AR40 etc.; In 3 grades, 1st-class, 2nd-class , 3rd-class; And 5 types in waterproof.. |
|||
Volume Resistivity | 0.0040 ohm-cm | 0.0040 ohm-cm | cured 2 hrs @ 65°C |
Tra-Con Tra-Duct 2907 Silver-Filled Epoxy Adhesive TRA-DUCT 2907 is an electrically conducting silver-filled medium viscosity epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical an.. |
|||
Volume Resistivity | 0.0040 ohm-cm | 0.0040 ohm-cm | Aged; Chomerics MAT-1002 |
Parker Chomerics CHO-FORM 5531 EMI Shielding Material One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. It is designed.. |
|||
Volume Resistivity | 0.0040 ohm-cm | 0.0040 ohm-cm | as supplied without pressure sensitive adhesive; MIL-DLT-83528 |
Parker Chomerics CHO-SEAL 1215 Conductive Elastomer Resists highest level of EMP induced current; military gasket of choice in non-corrosive environments; excellent processing for molding and extrusion. Molded and ExtrudedRoHS Compliant Information p.. |
|||
Volume Resistivity | <= 0.0040 ohm-cm | <= 0.0040 ohm-cm | |
Sinotek Materials R20 P Carbon Rod for Dry Battery We offer carbon rods for dry batteries in 11 regular sizes, including R03, R1, R6,R10, R12,R14, R20, R25, R40, S4, AR40 etc.; In 3 grades, 1st-class, 2nd-class , 3rd-class; And 5 types in waterproof.. |