Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | <= 0.050 ohm-cm | <= 0.050 ohm-cm | Mil-G-83528 |
P & P Technology EC-Q(F) Fluorosilicone Elastomer P & P Technology material reference EC-Q(F) is a fluorosilicone elastomer with a Nickel/Graphite conductive filler. Per MIL-G-83528. It is dark green in color. The material is specially compounded t.. |
|||
Volume Resistivity | <= 0.050 ohm-cm | <= 0.050 ohm-cm | DC |
Parker Chomerics CHO-BOND 1030 Conductive Silicone Gasket Adhesive Electrically conductive one-component silicone-based RTV adhesive which greatly simplifies the problem of bonding conductive silicone EMI gaskets to metal substrates. This adhesive cures on exposure.. |
|||
Volume Resistivity | 0.050 ohm-cm | 0.050 ohm-cm | R.T. cure |
Parker Chomerics CHO-BOND 589-29 Conductive Epoxy Low cost, highly conductive adhesive system which combines the strong adhesion characteristics of an epoxy with the superior conductivity of silver. CHO-BOND 589-29 adhesive meets the most exacting .. |
|||
Volume Resistivity | <= 0.050 ohm-cm | <= 0.050 ohm-cm | DC |
Parker Chomerics CHO-BOND 592 Conductive Epoxy Highly conductive silver-filled epoxy adhesive which combines the best properties of metals and organics. This two-component system is unique in that it combines long pot life, good electrical condu.. |
|||
Volume Resistivity | <= 0.050 ohm-cm | <= 0.050 ohm-cm | DC |
Parker Chomerics CHO-BOND® 592 Conductive Adhesive Description: CHO-BOND® 500 Series Adhesive/Sealant Compounds; These pure silver-filled materials are used where tight tolerances require thin bond lines. Various cure cycles are available, and the .. |
|||
Volume Resistivity | 0.050 ohm-cm | 0.050 ohm-cm | CEPS-0002 |
Parker Chomerics CHO-SEAL 1356 Conductive Elastomer Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con.. |
|||
Volume Resistivity | <= 0.050 ohm-cm | <= 0.050 ohm-cm | without pressure-sensitive adhesive; CEPS-0002 |
Parker Chomerics CHO-SEAL® 1270 Conductive Elastomer Description: Material of choice for high-end commercial applications; superior performance, in non-corrosive environments; tear trim compression and injection molding. A low durometer hardness elast.. |
|||
Volume Resistivity | 0.050 ohm-cm | 0.050 ohm-cm | as supplied (without psa); MIL-G-83528 |
Parker Chomerics CHO-SEAL® E6434E Conductive EPDM Elastomer Extruded Conductive EPDM Elastomer. This is an extruded conductive elastomer engineered for resistance to harsh chemicals, specifically those associated with decontaminates for military Nuclear, Bio.. |
|||
Volume Resistivity | <= 0.050 ohm-cm | <= 0.050 ohm-cm | |
Parker Chomerics Tecknit Consil®-V 751 Extruded Silver-Filled Silicone Elastomer Description: Consil-V is an extruded silicone elastomer filled with silver-plated inert particles. The V-shape cross section is ideally suited for applications requiring low closure force gasketing... |
|||
Volume Resistivity | 0.050 ohm-cm | 0.050 ohm-cm | Cured 12-24 hours at 25°C |
Resin Technology Group TIGA 920H Flexible Silver Conductive 100 parts resin to 115 parts hardener.TIGA 920-H is a flexible, conductive silver filled epoxy adhesive. It is recommended for bonding, and sealing electronic applications that require high flexibil.. |
|||
Volume Resistivity | 0.050 ohm-cm | 0.050 ohm-cm | Silicone Property; ASTM D991 |
Arlon Thermabond® 99730N004 0.004" (0.102 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Electrically Conductive - Thermabond®. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Coring.. |
|||
Volume Resistivity | 0.050 ohm-cm | 0.050 ohm-cm | Silicone Property; ASTM D991 |
Arlon Thermabond® 99730N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Electrically Conductive - Thermabond®. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Coring.. |
|||
Volume Resistivity | 0.050 ohm-cm | 0.050 ohm-cm | silicone property; ASTM D991 |
Arlon Thermabond® 99950N008 Silicone Rubber/Fiberglass Laminate Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |
|||
Volume Resistivity | 0.050 ohm-cm | 0.050 ohm-cm | silicone property; ASTM D991 |
Arlon Thermabond® 99950N015 Silicone Rubber/Fiberglass Laminate Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |
|||
Volume Resistivity | <= 0.050 ohm-cm | <= 0.050 ohm-cm | DC |
Parker Chomerics CHO-BOND 1035 Electrically Conductive Sealant Electrically conductive, one component RTV silicone which provides both environmental sealing and EMI/RFI shielding. This sealant, filled with silver-plated glass particles, contains no acetic acid,.. |
|||
Volume Resistivity | 0.050 ohm-cm | 0.050 ohm-cm | CHO MAT-1009 |
Parker Chomerics CHO-FORM 5538 Conductive Form-In-Place Gaskets Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |
|||
Volume Resistivity | 0.050 ohm-cm | 0.050 ohm-cm | cured 1 hr @ 100°C |
Tra-Con Tra-Duct 2929 Room Temperature Conductive Flexible Silver Epoxy Adhesive TRA-DUCT 2929 is recommended for electronic bonding, coating and sealing applications that require high flexibility coupled with excellent electrical and mechanical properties. This two-part epoxy a.. |