Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | 1V; IEC 60093 |
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | 1V; IEC 60093 |
Victrex® WG102™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PA6/6 CF20 L 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Semi Conductive and LubricatedInformation provided by TP C.. |
|||
Volume Resistivity | 1.00e+7 - 1.00e+11 ohm-cm | 1.00e+7 - 1.00e+11 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 0146 A Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Copper FillerFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+7 - 1.00e+11 ohm-cm | 1.00e+7 - 1.00e+11 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 0164 A Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Copper FillerFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Techmer ES Luriblend® PEI CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+7 - 1.00e+9 ohm-cm | 1.00e+7 - 1.00e+9 ohm-cm | ASTM D257 |
Techmer ES Statiblend® POM CO AS Availability: North AmericaForms: PelletsAdditive: AntistaticFeature: Antistatic and ConductiveTPCI# 60000114Information provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT G/CF30 15% Glass/Carbon Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 15% Filler by WeightAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Lubrizol Hipscon™ B-515 Static Control Polystyrene Hipscon™ B-515 is a carbon black-filled, Polystyrene compound available in compound form. Hipscom™ B-515 compound maintains extremely low gloss surfaces after molding, allowing for easy reading o.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | 50% RH; ASTM D257 |
Lubrizol Hipscon™ M-530 Static Control Polystyrene Hipscon™ M-530 is a conductive, carbon black filled, polystyrene available as extruded sheet and compound. Thermoformed trays are lightweight and easily formed into deep pockets that maintain unif.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Lubrizol Hipscon™ M-520 Static Control High Impact Polystyrene Hipscon™ M-520 is a conductive, carbon black filled, High Impact Polystyrene available as extruded sheet. Thermoformed trays are easily formed into deep pockets that maintain uniform static protec.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | IEC 60093 |
DSM Stanyl® TW200F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | IEC 60093 |
DSM Stanyl® TW271F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, PTFE Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | IEC 60093 |
DSM Stanyl® TW300 (COND) Nylon 46 Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Volume Resistivity | 1e+05 - 1.00e+7 ohm-cm | 1e+05 - 1.00e+7 ohm-cm | |
Diamond Polymers NPP25-0103 CF15 Conductive Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Volume Resistivity | 1e+05 - 1.00e+7 ohm-cm | 1e+05 - 1.00e+7 ohm-cm | ASTM D257 |
Clariant Renol PPSP0017 Polypropylene, Static Dissipative Data provided by Clariant Masterbatches |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Adamas Adalon® 103 PTFE, 10% Carbon Filled Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Adamas Adalon® 805 PTFE, 40% Bronze Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Adamas Adalon® 807 PTFE, 40% Bronze + 5 MoS2 Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Adamas Adalon® 812 PTFE, 46% Bronze, Green Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Adamas Adalon® 817 PTFE, 60% Bronze Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Adamas Adalon® 816 PTFE, 46% Bronze, Blue Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Techmer ES Statiblend® PPS GF35 SS7 BK 35/7% Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel Fiber, 35/7% Filler by WeightUL File Number: E157318Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | IEC 60093 |
DSM Stanyl® TW200F3 (COND) Nylon 46 15% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | 1V; IEC 60093 |
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |