Electrical Properties Metric English Comments
Volume Resistivity 1.50e+12 ohm-cm
1.50e+12 ohm-cm
ASTM D257
PolyOne Geon™ Vinyl Wire & Cable W1200 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Volume Resistivity 1.50e+12 ohm-cm
1.50e+12 ohm-cm
VDE 0303
GEHR Plastics POM-ESD-FG Polyoxymethylene
Variant of POM (Copolymer) with an improved electrical conductivity. Surface resistivity =1011 O. Polyoxymethylene can be used in temperatures ranging from -58 °F to +230 °F. The high surface..
Volume Resistivity 1.50e+12 ohm-cm
1.50e+12 ohm-cm
ASTM D257
PolyOne Geon™ Vinyl Wire & Cable W1100 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne