Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.90e+13 ohm-cm | 1.90e+13 ohm-cm | ASTM D247 |
Plenco 6310 Phenolic, Granular, Compression Molded PLENCO 06310 is a glass and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. 06310 is available in black.Information supplied by Plenco. |
|||
Volume Resistivity | 1.90e+13 ohm-cm | 1.90e+13 ohm-cm | IEC 60093 |
DSM Arnitel® XG5855 TPC-ET Extrusion Grade |