Polymer Property : Volume Resistivity = 3.60e+14 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 3.60e+14 ohm-cm
3.60e+14 ohm-cm
60°C for 500 hrs with 95% RH
Fujipoly Industries Sarcon® 85GSR Thin-Film GSR
Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of..
Volume Resistivity 3.60e+14 ohm-cm

@Temperature 70.0 °C
3.60e+14 ohm-cm

@Temperature 158 °F
7 days water immersion; IEC 60167
Lucobit Lucofin® 7410 HFFR EBA MDH Cable Sheathing
Lucofin® 7410 HFFR is a thermoplastic, halogen free flame retardant and low smoke compound for the insulation and/ or sheathing of cables. This grade is based on ethylene butyl acrylate (EBA) and..
Volume Resistivity 3.60e+14 ohm-cm

@Temperature 100 °C
3.60e+14 ohm-cm

@Temperature 212 °F
Tra-Con Tra-Bond 2126 Black Opaque Epoxy Adhesive
TRA-BOND 2126 is recommended for those modern photographic, industrial, and laboratory bonding and laminating applications where an easy-to-use, black (opaque) epoxy adhesive system with high perfor..
Volume Resistivity 3.60e+14 ohm-cm
3.60e+14 ohm-cm
3M Scotch-Weld™ EC-2086 Structural Adhesive
3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.Information provided by 3M