Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.90e+15 ohm-cm | 3.90e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti.. |
|||
Volume Resistivity | 3.90e+15 ohm-cm | 3.90e+15 ohm-cm | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 30GHR Thin-Film GHR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |