Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3000 ohm-cm | 3000 ohm-cm | 53 parts per 100 of NC E128-04 in the final compound |
Nanocyl EPOCYL™ NC E128-04 Master Batch Liquid Bisphenol-A Resin for Solvent Based Formulation Purposes EPOCYL™ NC E128-04 is a Mater Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl. It is specifically developed for so.. |
|||
Volume Resistivity | 3000 ohm-cm | 3000 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA)
(Unverified Data**) Ixef 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than glass-f.. |
|||
Volume Resistivity | 3000 ohm-cm | 3000 ohm-cm | |
LATI Latiohm 87/28-05 PD01 G/10 PC, 10% Glass Fiber Reinforced Semiconductive/dissipative product based on Polycarbonate (PC). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Volume Resistivity | 3000 ohm-cm | 3000 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA), 30% Carbon Fiber Ixef® 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than gla.. |
|||
Volume Resistivity | 3000 ohm-cm | 3000 ohm-cm | dry; IEC 60093 |
EMS-Grivory Grivory® GCL-3H anthracite PA*-CF30 Product description: Grivory GCL-3H anthracite is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is reinforced by 30% long ca.. |
|||
Volume Resistivity | 3000 ohm-cm | 3000 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® GCL-3H anthracite PA*-CF30 Product description: Grivory GCL-3H anthracite is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is reinforced by 30% long ca.. |
|||
Volume Resistivity | 3000 ohm-cm | 3000 ohm-cm | ISO 3915 |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |