Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nanocyl EPOCYL™ NC E128-04 Master Batch Liquid Bisphenol-A Resin for Solvent Based Formulation Purposes

Category Polymer , Thermoset , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Nanocyl
Trade Name EPOCYL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nanocyl EPOCYL™ NC E128-04 Master Batch Liquid Bisphenol-A Resin for Solvent Based Formulation Purposes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EPOCYL™ NC E128-04 is a Mater Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl. It is specifically developed for solvent based formulations to enhance the electrical conductivity of final epoxy formulations. Special features include easy integration and great flexibility in processing. Dilution factor has to be calculated accordingly to the desired level of conductivity.ApplicationsElectrostatic discharge (ESD) coatings, linings (tanks, rollers, ...) and compositesConductive primersResistive inksAdhesivesBenefitsLimited impact on base resin mechanical and thermo-mechanical propertiesEase of formulationOther information available upon request to NanocylCuring agents EPOCYL™ NCE128-04 based formulations can be cured or cross-linked with different types of curing agents which could be decided accordingly to the desired processing conditions and the properties of the final composite like any conventional Bis-A based formulations.
Physical Properties Metric English Comments
Specific Gravity 1.15 - 1.20 g/cc
1.15 - 1.20 g/cc
Viscosity 25000 - 45000 cP

@Temperature 25.0 °C
25000 - 45000 cP

@Temperature 77.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 3000 ohm-cm
3000 ohm-cm
53 parts per 100 of NC E128-04 in the final compound
20000 ohm-cm
20000 ohm-cm
26 parts per 100 of NC E128-04 in the final compound
70000 ohm-cm
70000 ohm-cm
13 parts per 100 of NC E128-04 in the final compound
Descriptive Properties Value Comments
Aspect Paste, black (Master Batch)
Epoxy Equivalent 196.1 - 203.52 g/eq
Epoxy Value 4.91 - 5.1 eq/kg
Storage Temperature 5°C - 40°C