Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.0 - 5.0 ohm-cm | 1.0 - 5.0 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ CTX 1125 PC/ABS Blend, Carbon Fiber Reinforced
(discontinued **) Description/Features:Electrically ConductiveNickel Coated Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |