Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+15 - 5.00e+15 ohm-cm | 1.00e+15 - 5.00e+15 ohm-cm | IEC 60093 |
Polycasa AKRYLON XT PMMA AKRYLON XT sheets have good optical properties and high quality surfaces. AKRYLON XT sheets also show excellent color and functional stability and can be used in contact with foodstuffs. AKRYLON XT .. |
|||
Volume Resistivity | 1.00e+15 - 5.00e+15 ohm-cm | 1.00e+15 - 5.00e+15 ohm-cm | IEC 60093 |
Polycasa XT PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |