Polymer Property : Volume Resistivity = 500000 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 500000 ohm-cm
500000 ohm-cm
LATI Latiohm 36/07 PD01 G/20 ABS, 20% Glass Fiber Reinforced
Semiconductive/dissipative product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfor..
Volume Resistivity 500000 ohm-cm
500000 ohm-cm
IEC 60093
Borealis FR4810 Low Smoke Zero Halogen Flame Retardant Jacketing Compound
FR4810 is a thermoplastic, low smoke zero halogen (LSZH) flame retardant, black jacketing compound combining with flexibility and exceptional fluid resistance. The composition is based on the elemen..