Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 6.20e+11 ohm-cm | 6.20e+11 ohm-cm | ASTM D247 |
Plenco 6582 Phenolic, Briquette, Transfer Molded PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo.. |
|||
Volume Resistivity | 6.20e+11 ohm-cm | 6.20e+11 ohm-cm | |
3M Safety-Walk™ 5100 Cushion Matting The product is a durable, flexible, vinyl mat having an open construction for easy, cleaning, comfort and safety. The mat has a low profile to minimize interference with foot and cart traffic. The v.. |