Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 6600 ohm-cm | 6600 ohm-cm | EVA/NBR Strippable Compounds |
TIMCAL ENSACO™ 210G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |
|||
Volume Resistivity | 6600 ohm-cm | 6600 ohm-cm | |
LATI Latimass 82-05 D040 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |