Volume Resistivity 7.10e+11 ohm-cm
7.10e+11 ohm-cm
ASTM D247
Plenco 4548 Phenolic, Granular, Transfer Molded
PLENCO 04548 is a heat resistant mineral filled phenolic molding compound, offering fast cure rates and hot rigidity. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04548 is avai..