Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Volume Resistivity = 7.40e+13 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 7.40e+13 ohm-cm
7.40e+13 ohm-cm
60°C for 500 hrs
Fujipoly Industries Sarcon® 45T Thin-Film TR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Volume Resistivity 7.40e+13 ohm-cm
7.40e+13 ohm-cm
60°C for 1,000 hrs with 90% RH; JIS-K-6249
Fujipoly Industries Sarcon® GR-d Gap Filler Pad
Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries
Volume Resistivity 7.40e+13 ohm-cm
7.40e+13 ohm-cm
ASTM D257
Arkema Group Orgalloy® LT 5050 Polyamide Alloy
Polyamide Alloy, Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
Volume Resistivity 7.40e+13 ohm-cm
7.40e+13 ohm-cm
ASTM D257
Arkema Group Orgalloy® LT 5050 ES Polyamide Alloy
Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group
Volume Resistivity 7.40e+13 ohm-cm
7.40e+13 ohm-cm
E24/125; IPC TM-650 2.5.17.1
Arlon 47N Quick Cure Epoxy Low-Flow Prepreg
47N is a low-flow epoxy prepreg engineered for binding multilayer epoxy rigid-flex or attaching heat sinks to multilayer PCBs. An optional low lamination temperature protects components already mou..
Copyright © lookpolymers.com All Rights Reserved