Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 7.50e+13 ohm-cm | 7.50e+13 ohm-cm | ASTM D247 |
Plenco 00714 Melamine-Phenolic, Granular, Compression Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |