Polymer Property : Volume Resistivity = 8.00e+10 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+10 ohm-cm
8.00e+10 ohm-cm
LATI Latiohm 62-08 PD02 G/30 PPA, 30% Glass Fiber Reinforced
Dissipative product based on Polyamide 6 (PA6). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Volume Resistivity 8.00e+10 ohm-cm
8.00e+10 ohm-cm
ASTM D257
Lubrizol Stat-Rite® M-690 Static Control PETG Alloy
Stat-Rite® M-690 is a static dissipative PETG alloy. Stat-Rite® M-690 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protectio..
Volume Resistivity 8.00e+10 ohm-cm
8.00e+10 ohm-cm
ASTM D247
Plenco 5488 Phenolic, Granular, Injection Molded
PLENCO 05488 is a woodflour and graphite filled phenolic molding compound offering improved abrasion resistance. UL recognized under component file E40654. 05488 is available in brown. 05488 is not ..