Polymer Property : Volume Resistivity = 8.00e+6 ohm-cm
Polymer Property :
Volume Resistivity =
8.00e+6 ohm-cm
Product List
Electrical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties
Metric
English
Comments
Volume Resistivity
8.00e+6
ohm-cm
8.00e+6
ohm-cm
IEC 93
Micropol Microstat ML21 Linear medium density static dissipative polyethylene
Information provided by Micropol Limited