Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Micropol Microstat ML21 Linear medium density static dissipative polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Micropol Limited
Trade Name Microstat
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Micropol Microstat ML21 Linear medium density static dissipative polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Micropol Limited
Physical Properties Metric English Comments
Density 0.936 g/cc
0.0338 lb/in³
ASTM D792-91
Melt Flow 7.0 - 9.0 g/10 min
7.0 - 9.0 g/10 min
ASTM D1238-94
Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.0 MPa
2320 psi
50mm/min; ASTM D638M-89
Elongation at Break 350 %
350 %
ASTM D638-M89
Flexural Modulus 0.560 GPa
81.2 ksi
ASTM D790-M86
Izod Impact, Notched 0.900 J/cm

@Temperature -20.0 °C
1.69 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Vicat Softening Point 111 °C
232 °F
5 kilo load; ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+6 ohm-cm
8.00e+6 ohm-cm
IEC 93
Surface Resistance 2.20e+7 ohm
2.20e+7 ohm
IEC 93
Users viewing this material also viewed the following: