Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 9.70e+14 ohm-cm | 9.70e+14 ohm-cm | ASTM D257 |
Teknor Apex HFFR 2005 Polyolefin, Halogen Free Notes: RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable Jacketing; Plenum Cable JacketingAgency Ratings: IEC Unsp.. |