Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 9.80e+7 ohm-cm | 9.80e+7 ohm-cm | ASTM D257 |
Zircar Refractory Composites ZIRCAL-45 Refractory Board Type ZIRCAL-45 Refractory Board is a self supporting, high strength, rigid refractory product fabricated from calcium silicate, inert fillers and reinforcing agents. Its high structural strength com.. |
|||
Volume Resistivity | 9.80e+7 ohm-cm | 9.80e+7 ohm-cm | ASTM D257 |
BNZ Materials Marinite® I&M High Temperature Structural Insulation Oven dried formulations of BNZ boards are used in a variety of heat insulating processes, fire protection and machined parts. Selection is commonly based on a balance between strength and insulating.. |