Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 - 1.00e+12 ohm-cm

@Temperature 1000 °C
1.00e+10 - 1.00e+12 ohm-cm

@Temperature 1830 °F
China-Yixing Longly Refractories Steatite Ceramics (High Frequency Porcelain)
LONGLY's steatite ceramics (namely high frequency porcelain, strengthened porcelain, magnesia porcelain), molecular formula as MgO-SiO2, is pure white. Steatite is the appropriate option when good ..