Volume Resistivity 1.00e+16 ohm-cm

@Temperature 23.0 °C
1.00e+16 ohm-cm

@Temperature 73.4 °F
Result based on 450G
Victrex® PEEK 600G Polyetheretherketone  (discontinued **)
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta..
Volume Resistivity 1.00e+16 ohm-cm

@Temperature 23.0 °C
1.00e+16 ohm-cm

@Temperature 73.4 °F
IEC 60093
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c..
Volume Resistivity 1.00e+16 ohm-cm

@Temperature 23.0 °C
1.00e+16 ohm-cm

@Temperature 73.4 °F
IEC 60093
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou..
Volume Resistivity 1.00e+16 ohm-cm

@Temperature 23.0 °C
1.00e+16 ohm-cm

@Temperature 73.4 °F
IEC 60093
Victrex® PEEK 450G General Purpose
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac..
Volume Resistivity 1.00e+16 ohm-cm

@Temperature 23.0 °C
1.00e+16 ohm-cm

@Temperature 73.4 °F
IEC 60093
Victrex® PEEK 90G Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c..
Volume Resistivity 1.00e+16 ohm-cm

@Temperature 23.0 °C
1.00e+16 ohm-cm

@Temperature 73.4 °F
IEC 60093
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia..
Volume Resistivity >= 1.00e+16 ohm-cm

@Temperature 75.0 °C
>= 1.00e+16 ohm-cm

@Temperature 167 °F
Master Bond EP112M Two Component, Medium Viscosity Heat Curing Cycloaliphatic Epoxy Resin
Product Description: Master Bond Polymer System EP112M is a solventless, medium viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor ..
Volume Resistivity 1.00e+16 ohm-cm

@Temperature 25.0 °C
1.00e+16 ohm-cm

@Temperature 77.0 °F
DC100V; ASTM D257
UBE UPILEX 75S (75 micron) Polyimide Film
Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries..
Volume Resistivity 1.00e+16 ohm-cm

@Temperature 200 °C
1.00e+16 ohm-cm

@Temperature 392 °F
DC100V; ASTM D257
UBE UPILEX 75S (75 micron) Polyimide Film
Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries..
Volume Resistivity 1.00e+16 ohm-cm

@Temperature 25.0 °C
1.00e+16 ohm-cm

@Temperature 77.0 °F
Abatron AboCast 7703-21/AboCure 7703-21 (A) Epoxy Adhesive and Casting Compound
AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane..
Volume Resistivity 1.00e+16 ohm-cm

@Temperature 23.0 °C
1.00e+16 ohm-cm

@Temperature 73.4 °F
Results based on HT G22
Victrex® HT™ G45 Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia..
Volume Resistivity 1.00e+16 ohm-cm

@Temperature 23.0 °C
1.00e+16 ohm-cm

@Temperature 73.4 °F
Victrex® PEEK 650G Polyetheretherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta..
Volume Resistivity 1.00e+16 ohm-cm

@Temperature 23.0 °C
1.00e+16 ohm-cm

@Temperature 73.4 °F
IEC 60093
Victrex® PEEK 381G Medium Viscosity
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD..
Volume Resistivity 1.00e+16 ohm-cm

@Temperature 23.0 °C
1.00e+16 ohm-cm

@Temperature 73.4 °F
IEC 60093
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac..