Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.60e+11 ohm-cm @Temperature 250 °C |
1.60e+11 ohm-cm @Temperature 482 °F |
|
Schott Glass 8651 Sealing Glass Tungsten sealing glass Power diodesInformation provided by SCHOTT AG. |
|||
Volume Resistivity | 1.60e+11 ohm-cm @Temperature 250 °C |
1.60e+11 ohm-cm @Temperature 482 °F |
|
Corning Pyrex® 7740 Borosilicate Glass Pyrex® sheet provides unique chemical, thermal, mechanical, and optical properties. Available in thicknesses from 3/32 inches to 2.25 inches. Tempering increases temperature and pressure capabili.. |