Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.00e+12 ohm-cm @Temperature 23.0 °C |
2.00e+12 ohm-cm @Temperature 73.4 °F |
50%RH; IEC 60093 |
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66
(Unverified Data**) Zytel® FE270038 is a 40% glass fiber/mineral reinforced, heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.Information provided by DuPont Performan.. |