Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 50 ohm-cm @Temperature 23.0 °C |
50 ohm-cm @Temperature 73.4 °F |
ASTM D991 |
Borealis LE0310-44 Polyethylene Compound, Crosslinkable, Semiconductive LE0310-44 is a strippable semi conductive insulation shield for insulated, medium voltage (5-46kV) cables. Strip force range from 7 to 14 lbs/0.5". Specifications: NF C33-223; UTE C 33-223; AEIC CS.. |
|||
Volume Resistivity | 50 ohm-cm @Temperature 23.0 °C |
50 ohm-cm @Temperature 73.4 °F |
ASTM D991 |
Borealis LE0310-99 Polyethylene Thermoplastic Semiconductive Compound LE0310-99 has the same melt flow properties as the peroxide containing material. Application: LE0310-99 is used during start up of a triple-head line. It helps to use a non-peroxide-containing mate.. |
|||
Volume Resistivity | 50 ohm-cm @Temperature 23.0 °C |
50 ohm-cm @Temperature 73.4 °F |
ASTM D991 |
Borealis LE0315-99 Polyethylene Thermoplastic Semiconductive Compound LE0315-99 has the same melt flow properties as the peroxide containing material. Application: LE0315-99 is used during start up of a triple-head line. It helps to use a non-peroxide containing mate.. |
|||
Volume Resistivity | <= 50 ohm-cm @Temperature 23.0 °C |
<= 50 ohm-cm @Temperature 73.4 °F |
ISO 3915 |
Borealis LE0563 Polyethylene Compound, Thermoplastic, Semiconductive LE0563 is a thermoplastic semi conductive compound specifically designed for medium- and high voltage cable systems requiring improved grounding. It may be used either as a complete jacket or as a t.. |