Borealis LE0310-44 Polyethylene Compound, Crosslinkable, Semiconductive

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Borealis
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis LE0310-44 Polyethylene Compound, Crosslinkable, Semiconductive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LE0310-44 is a strippable semi conductive insulation shield for insulated, medium voltage (5-46kV) cables. Strip force range from 7 to 14 lbs/0.5". Specifications: NF C33-223; UTE C 33-223; AEIC CS8-00 (1st edition); IEC 60502; ICEA S-97-682; BS 6622; ICEA S-94-649; and NF C33-223.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.0 MPa
1890 psi
ASTM D638
Elongation at Break >= 75 %
>= 75 %
after aging 7days @ 136°C; ASTM D638
300 %
300 %
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature <= -35.0 °C
<= -31.0 °F
ASTM D746
Electrical Properties Metric English Comments
Volume Resistivity 50 ohm-cm

@Temperature 23.0 °C
50 ohm-cm

@Temperature 73.4 °F
ASTM D991
90 ohm-cm

@Temperature 90.0 °C
90 ohm-cm

@Temperature 194 °F
ASTM D991
Processing Properties Metric English Comments
Processing Temperature <= 230 °C
<= 446 °F
cable surface temperature in curing tube
Shelf Life 12.0 Month
12.0 Month