Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 6.70e+14 ohm-cm @Temperature 20.0 °C |
6.70e+14 ohm-cm @Temperature 68.0 °F |
IEC 60502 |
Solvay Specialty Polymers Cogegum® GFR/350 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Volume Resistivity | 6.70e+14 ohm-cm @Temperature 20.0 °C |
6.70e+14 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Solvay Specialty Polymers Cogegum® GFR/350 Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a pol.. |
|||
Volume Resistivity | 6.70e+14 ohm-cm @Temperature 23.0 °C |
6.70e+14 ohm-cm @Temperature 73.4 °F |
50%RH; IEC 60093 |
DuPont Performance Polymers Zytel® PLUS PLS95G35DH1 BK031 Nylon Zytel® PLS95G35DH1 BK031is a high flow 35% glass reinforced PA using SHIELD Technology, only from DuPont, combining excellent surface appearance, excellent welding and fatigue retention, exceptiona.. |