Solvay Specialty Polymers Cogegum® GFR/350 Polyolefin

Category Polymer , Thermoplastic , Polyolefin
Manufacturer Solvay Specialty Polymers
Trade Name Cogegum®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Cogegum® GFR/350 Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefin base containing a fire retardant system that contributes to give the cable self-extinguish properties without halogenidric acids evolution, toxic and corrosive gases and dark smoke emission. Features: Crosslinkable; Flame Retardant; Halogen Free; Low Smoke Emission; Low Toxicity; Self ExtinguishingUses: Cable Jacketing; Low Voltage Insulation; Wire & Cable ApplicationsAdditional Properties: Bending Test - IEC 60811 (-15°C): No cracks; Calorific Potential - ISO 1716 18.6 MJ/kg; Collar Temperature - 160 to 180 °C; Corrosive Gas in Smoke - IEC 60754-2 < 10.0 µS/mm; Corrosive Gas in Smoke - IEC 60754-2 > 4.30; Halogenidric Acid Emissions - IEC 60754-1 < 0.10 %; Head Temperature - 160 to 180 °C; Hot Air Shrinkage - IEC 60811 (100°C): < 4.0 %; Hot Pressure Test - IEC 60811 (100°C): < 50 %; Hot Set - IEC 60811 50 %; Hot Set - IEC 60811 0.0 %; Impact Test - IEC 60811 (-15°C): No cracks; Insulation Resistance Constant - IEC 60502 (20°C): 2500 Mohm·km; Insulation Resistance Constant - IEC 60502 (90°C): 200 Mohm·km; Temperature Index (Burning) - NES 715 300 °C; Water Absorption - IEC 60811 (100°C): < 4.00 mg/cm²Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded, 10% Igepal; ASTM D1693
Melt Flow 3.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
3.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 38
38
ISO 868
Tensile Strength at Break 12.3 MPa
1780 psi
ASTM D638
Elongation at Break 210 %
210 %
ASTM D638
Thermal Properties Metric English Comments
Oxygen Index 38 %
38 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 5.40e+13 ohm-cm

@Temperature 90.0 °C
5.40e+13 ohm-cm

@Temperature 194 °F
ASTM D257
6.70e+14 ohm-cm

@Temperature 20.0 °C
6.70e+14 ohm-cm

@Temperature 68.0 °F
ASTM D257
Processing Properties Metric English Comments
Zone 1 120 - 140 °C
248 - 284 °F
Zone 2 130 - 150 °C
266 - 302 °F
Zone 3 140 - 160 °C
284 - 320 °F
Zone 4 150 - 170 °C
302 - 338 °F
Die Cooling Temperature 180 - 210 °C
356 - 410 °F
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
RoHS Compliance RoHS Compliant