Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 200 V @Temperature 23.0 °C |
200 V @Temperature 73.4 °F |
IEC 60112 |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Comparative Tracking Index | 200 V @Temperature 23.0 °C |
200 V @Temperature 73.4 °F |
IEC 60112 |
DuPont Performance Polymers Rynite® GW520CS NC010 PET
(Unverified Data**) Rynite® GW520CS NC010 is a 20% glass fiber reinforced, flame retardant, color stabilized, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |