Electrical Properties Metric English Comments
Comparative Tracking Index 250 V

@Thickness 3.20 mm
250 V

@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
Nilit Nilitop BT FR C3 Unfilled, Flame Retardant PBT
Description: Nilitop BT FR C3 is an unfilled, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive.Key characteristics: Go..
Comparative Tracking Index 250 V

@Thickness 3.20 mm
250 V

@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
Nilit Nilitop BT G2 FR C3 is a 10% Glass Fiber Reinforced, Flame Retardant PBT
Description: Nilitop BT G2 FR C3 is a 10% glass fiber reinforced, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive. It..
Comparative Tracking Index 250 V

@Thickness 3.20 mm
250 V

@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
Nilit Nilitop BT G4 FR C3 is a 20% Glass Fiber Reinforced, Flame Retardant PBT
Description: Nilitop BT G4 FR C3 is a 20% glass fiber reinforced, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive. It..
Comparative Tracking Index 250 V

@Thickness 3.20 mm
250 V

@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
Nilit Nilitop BT G6 FR C3 is a 30% Glass Fiber Reinforced, Flame Retardant PBT
Description: Nilitop BT G6 FR C3 is a 30% glass fiber reinforced, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive. It..
Comparative Tracking Index 250 V

@Temperature 23.0 °C
250 V

@Temperature 73.4 °F
UL 746A
DuPont Performance Polymers Crastin® S600F20 BK851 PBT  (Unverified Data**)
Crastin® S600F20 BK851 is an unreinforced, lubricated, medium viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 250 V

@Temperature 23.0 °C
250 V

@Temperature 73.4 °F
UL 746A
DuPont Performance Polymers Crastin® S600F20 NC010 PBT  (Unverified Data**)
Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 250 V

@Temperature 23.0 °C
250 V

@Temperature 73.4 °F
UL 746A
DuPont Performance Polymers Crastin® S600F40 NC010 PBT  (Unverified Data**)
Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 250 V

@Temperature 23.0 °C
250 V

@Temperature 73.4 °F
UL 746A
DuPont Performance Polymers Crastin® S620F20 BK851 PBT  (Unverified Data**)
Crastin® S620F20 BK851 is an unreinforced, nucleated, lubricated, medium viscosity, black polybutylene terephthalate resin for fast injection molding.Information provided by DuPont Performance Poly..
Comparative Tracking Index 250 V

@Temperature 23.0 °C
250 V

@Temperature 73.4 °F
UL 746A
DuPont Performance Polymers Crastin® SK601 BK851 PBT  (Unverified Data**)
Crastin® SK601 BK851 is a 10% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 250 V

@Temperature 23.0 °C
250 V

@Temperature 73.4 °F
UL 746A
DuPont Performance Polymers Rynite® FR530 BK507 PET  (Unverified Data**)
Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Comparative Tracking Index 250 - 400 V

@Temperature 23.0 °C
250 - 400 V

@Temperature 73.4 °F
UL 746A
DuPont Performance Polymers Rynite® FR530 BK507 PET  (Unverified Data**)
Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Comparative Tracking Index 250 V

@Temperature 23.0 °C
250 V

@Temperature 73.4 °F
UL 746A
DuPont Performance Polymers Rynite® FR530L BK507 PET  (Unverified Data**)
Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Comparative Tracking Index 250 - 400 V

@Temperature 23.0 °C
250 - 400 V

@Temperature 73.4 °F
UL 746A
DuPont Performance Polymers Rynite® FR530L BK507 PET  (Unverified Data**)
Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Comparative Tracking Index 250 V

@Temperature 23.0 °C
250 V

@Temperature 73.4 °F
UL 746A
DuPont Performance Polymers Rynite® GW520CS NC010 PET  (Unverified Data**)
Rynite® GW520CS NC010 is a 20% glass fiber reinforced, flame retardant, color stabilized, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Comparative Tracking Index 250 V

@Temperature 23.0 °C
250 V

@Temperature 73.4 °F
DAM; UL 746A
DuPont Performance Polymers Zytel® 70G35HSL BK039B Nylon 66  (Unverified Data**)
Zytel® 70G35HSL BK039B is a 35% glass fiber reinforced, heat stabilized, black polyamide 66 for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 250 - 400 V

@Temperature 23.0 °C
250 - 400 V

@Temperature 73.4 °F
DAM; UL 746A
DuPont Performance Polymers Zytel® 70G35HSL BK039B Nylon 66  (Unverified Data**)
Zytel® 70G35HSL BK039B is a 35% glass fiber reinforced, heat stabilized, black polyamide 66 for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 250 - 400 V

@Thickness 1.50 mm
250 - 400 V

@Thickness 0.0591 in
DAM; UL 746A
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66  (Unverified Data**)
Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 250 - 400 V

@Thickness 0.750 mm
250 - 400 V

@Thickness 0.0295 in
DAM; UL 746A
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66  (Unverified Data**)
Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 250 - 400 V

@Thickness 3.00 mm,
Temperature 23.0 °C
250 - 400 V

@Thickness 0.118 in,
Temperature 73.4 °F
DAM; UL 746A
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66  (Unverified Data**)
Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 250 - 400 V

@Thickness 1.00 mm,
Temperature 23.0 °C
250 - 400 V

@Thickness 0.0394 in,
Temperature 73.4 °F
DAM; UL 746A
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66  (Unverified Data**)
Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 250 - 400 V

@Temperature 23.0 °C
250 - 400 V

@Temperature 73.4 °F
DAM; IEC 60112
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 250 - 400 V

@Temperature 23.0 °C
250 - 400 V

@Temperature 73.4 °F
50%RH; IEC 60112
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 250 - 400 V

@Temperature 23.0 °C
250 - 400 V

@Temperature 73.4 °F
DAM; UL 746A
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 250 - 400 V

@Thickness 3.00 mm,
Temperature 23.0 °C
250 - 400 V

@Thickness 0.118 in,
Temperature 73.4 °F
DAM; UL 746A
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers