Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 279 kV/in Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Dielectric Strength 11.0 kV/mm
279 kV/in
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data)
Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig..
Dielectric Strength 11.0 kV/mm
279 kV/in
Permabond HH167 Anaerobic Retainer
Permabond® HH167 is a high viscosity gap filling silver paste, which can be used for repairing metal machinery parts. It is ideal for repairing worn shafts, broken threads, damaged keyways and spli..
Dielectric Strength 11.0 kV/mm
279 kV/in
Permabond HL138 Anaerobic Retaining Compound
Permabond® HL138 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure which ..
Dielectric Strength 11.0 kV/mm
279 kV/in
Permabond HM118 Anaerobic Threadlocker
Permabond® HM118 Threadlocker is an excellent general-purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Cure is fast and reliable on s..
Dielectric Strength 11.0 kV/mm
279 kV/in
Permabond HM129 Anaerobic Threadlocker
Permabond® HM129 is a high strength medium viscosity anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. Cure is fast and reliable on st..
Dielectric Strength 11.0 kV/mm
279 kV/in
Permabond HM161 Anaerobic Retaining Compound
Permabond® HM161 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space’ between parts and upon cure unitiz..
Dielectric Strength 11.0 kV/mm
279 kV/in
Permabond HM162 Anaerobic Retainer
Permabond® HM162 is a medium viscosity retaining compound that cures when confined between metal parts to form an extremely tough bond. It is best suited for cylindrical parts and where high temper..
Dielectric Strength 11.0 kV/mm
279 kV/in
Permabond HM165 Anaerobic Retainer
Permabond® HM165 is a high viscosity anaerobic retaining compound that cures when confined between metal parts to form a tough bond. It is best suited for cylindrical parts and where high temperatu..
Dielectric Strength 11.0 kV/mm
279 kV/in
Permabond LH197 Anaerobic Gasketmaker
Permabond® LH197 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is highly flexible, making it ideal for dissimilar surfaces where differential th..
Dielectric Strength 11.0 kV/mm
279 kV/in
JIS-K-6249; ASTM D-149
Fujipoly Industries Sarcon® NR-c Gap Filler Pad Non-Silicone
Sarcon NR-c consists of an Acrylate resin and some thermal conductive fillers. It is a highly conformable/ thermally conductive material in a versatile sheet form that makes reliable and complete p..
Dielectric Strength 11.0 kV/mm
279 kV/in
Saint-Gobain Micaver® Glass-Mica Electrical Insulator, Transfer Moldings
Glass-mica compound that occupies a place between plastics and ceramics in terms of usage temperature. It can be molded and machined like plastics and has the mechanical properties (strength, hardn..
Dielectric Strength 11.0 kV/mm
279 kV/in
Short Time; ASTM D149
Plenco 3356 Phenolic, Granular, Injection Molded
PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i..
Dielectric Strength 11.0 kV/mm
279 kV/in
ASTM D149; at 1 mil
Westlake Plastics HTP 800 Clear PVC
HTP 800 is a clear PVC based material for use as windows and doors in cleanroom equipment. Notable properties include light transmission, chemical resistance, and flame resistance. Information prov..
Dielectric Strength 11.0 kV/mm
279 kV/in
Short Time; ASTM D149
Plenco 4311 Phenolic, Granular, Injection Molded
PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized..
Dielectric Strength 11.0 kV/mm
279 kV/in
ASTM D149
Toyobo TS201 HS PPS, Glass Fiber/Mineral Reinforced
Key Feature: High stiffness, high toughnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excel..
Dielectric Strength 11.0 kV/mm
279 kV/in
Dow Corning SE 4448 CV KIT PARTS A&B
Excellent thermal conductivity, low volatility (D4-D10 0.03% wt), heat cure, high viscosity.Information provided by Dow Corning
Dielectric Strength 11.0 kV/mm
279 kV/in
Dow Corning SLYGARD® 535 THIXOTROPIC DIELECTRIC GEL
Information provided by Dow Corning
Dielectric Strength 11.0 kV/mm

@Thickness 3.00 mm
279 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes
Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength. Retains electrical properties at high air humidity. High resistance to chemicals.Applications..
Dielectric Strength 11.0 kV/mm

@Thickness 3.00 mm
279 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Tubes
Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength, even at high temperatures. Retains electrical properties at high air humidity. High resistanc..
Dielectric Strength 11.0 kV/mm

@Thickness 3.00 mm
279 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Elektro-Isola G-Etronax EP 22 Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes
Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength, even at high temperatures. Retains electrical properties at high air humidity. High resistanc..
Dielectric Strength 11.0 kV/mm
279 kV/in
Permabond A011 Anaerobic Threadlocker
Permabond® A011 is an anaerobic adhesive designed for locking and sealing threaded or coaxially fitting metal parts where subsequent dismantling is required. Its controlled strength ensures fatigue..
Dielectric Strength 11.0 kV/mm
279 kV/in
Permabond HM135 Anaerobic Retainer
Permabond® HM135 is a fast curing, medium viscosity anaerobic adhesive for locking and sealing threads and retaining cylindrical components. It gives maximum torque strength on brass or plated bras..
Dielectric Strength 11.0 kV/mm
279 kV/in
Permabond MH052 Anaerobic Threadsealant
Permabond® MH052 is ideal for the sealing of threaded joints. It is approved for use with natural gas and LPG for working pressure up to 20 bar (290 psi) and also for gaseous oxygen up to 10 bar (1..
Dielectric Strength 11.0 kV/mm
279 kV/in
ASTM D149
Plaslok 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 5000 is the replacement material for ..
Dielectric Strength 11.0 kV/mm
279 kV/in
Permabond A1046 Anaerobic Retainer
Permabond® A1046 is a rapid curing adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, pulleys and threaded components. It exhibits high strength and ..
Dielectric Strength 11.0 kV/mm
279 kV/in
Permabond A118 Anaerobic Retainer
Permabond® A118 is an anaerobic adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, studs and other threaded components. It exhibits high strength, ex..
Dielectric Strength 11.0 kV/mm
279 kV/in
Permabond A130 Anaerobic Threadlocker
Designed for the locking and sealing of metal parts, Permabond® A130 is ideally suited for use on components that need to be dismantled for maintenance. Giving vibration resistance it can be used t..
Copyright © lookpolymers.com All Rights Reserved