3M™ Fast Tack Water Based Adhesive 1000NF is a high performance water-based, one part adhesive formulated for fast bonding and long term heat resistant bonds.Information provided by 3M
Physical Properties Metric English Comments
Density 0.959 - 1.08 g/cc
0.0346 - 0.0390 lb/in³
Solids Content 46 - 51 %
46 - 51 %
Brookfield Viscosity 400 - 1100 cP
400 - 1100 cP
RVF 3# sp @ 30 rpm, RT
Descriptive Properties Value Comments
Appearance Neutral, Purple
Base Acrylic Emulsion