Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.959 g/cc | 0.0346 lb/in³ | ISO 1183 |
SABIC P6006 Black High Density Polyethylene for Pipes Product Description: P6006 is a black compound high density (class MRS 8 - PE 80) polyethylene with bimodal distribution of molecular mass. It is specifically designed for Pressure Pipe applicatio.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM D 792 |
NOVA Chemicals Novapol® HE-W959-A HDPE Extrusion/Blow Molding Resin HE-W959-A complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolog.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ISO 1183 |
Total Finathene® 6002 HDPE, blow molding, pipe
(discontinued **) FINATHENE® 6002 is a high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® 6002 has been especially developed for the manufacturing of toys and of b.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM D 792 |
Total Finathene® 1288 HDPE film
(discontinued **) Applications: Flat bottom bags, draw strings, coextruded merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plasti.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM D 792 |
Total Finathene® 7208 HDPE extrusion resin
(discontinued **) Applications: monofilament, slit tape, woven and knitted fabrics, specialty filmsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics .. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM D1475 |
Humiseal 1A27 Urethane Conformal Coating Humiseal 1A27 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedPasses thermal shock test (MIL-I-46058C)Flammabilit.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM D1475 |
Humiseal 1B73LSE Acrylic Conformal Coating Humiseal 1B73LSE Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityUL Approval PendingMIL-I-46058C Approval Pendin.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM D1475 |
Humiseal 1C61 UV Cure Conformal Coating Humiseal 1C61 UV Cure Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock t.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM D1475 |
Humiseal 1C65 Silicone Conformal Coating Humiseal 1C65 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM D792 |
LyondellBasell Alathon® L5906 High Density Polyethylene ApplicationsALATHON XL 5906 is a high molecular weight high density polyethylene homopolymer with a broad bimodal molecular weight distribution. This resin exhibits excellent stiffness, very high t.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ISO 1183 |
FKuR Kunststoff Terralene® HD 3505 Biobased Polyethylene With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Black; ASTM D4883 |
Ineos TUB 121 HDPE TUB 121 (aka ELTEX® TUB 121, ELTEX® TUB 121 N2025, and ELTEX® TUB 121 N3000) is a black high density bimodal polyethylene copolymer designed for extrusion of potable water, natural gas, ind.. |
|||
Density | 0.959 - 0.965 g/cc | 0.0346 - 0.0349 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GD 5160 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.959 - 1.01 g/cc | 0.0346 - 0.0364 lb/in³ | |
Lord Adhesives 551 Very Low Viscosity, Adhesive Thinner, Medium Cure Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) BL 3VD HH 4765 High Density Polyethylene BL3VD is a high density polyethylene with 1-Butene as co monomer. It is very high density and stiffness, good ESCR, high flowability and impact strength.Applications: small blow molding, bottles, c.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA555 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low exotherm adhesive able to be used 1" thick.Information provided by Illinois Tool Works. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Compound; ISO 1183 |
Borealis BorPEX™ HE2558 Blue High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide)) BorPEX HE2558 is a blue, high molecular weight, high density polyethylene compound for crosslinkable pipes, specially designed for peroxide crosslinking. Long stability and UV resistance is ensured.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | compound; ISO 1872-2/ISO 1183 |
Borealis BorSafe™ HE3490-LS-H HDPE Compound for Pressure Pipes BorSafe™ HE3490-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal s.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ISO 1183 |
Total Xsene® BM 593 HDPE, blow molding FINATHENE® BM 593 is a new generation of bimodal high density polyethylene based on hexene (C6) as co-monomer and is produced by the ATOFINA Double Loop Technology™. FINATHENE® BM 593 has been es.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM D 792 |
Total Xsene® XS10 B HDPE, pipe, injection molding FINATHENE® XS10 B is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS10 B is a high performance black compound speci.. |
|||
Density | 0.959 - 0.963 g/cc | 0.0346 - 0.0348 lb/in³ | ASTM D4052 |
ExxonMobil Jayflex™ DIUP Plasticizer (European Grade) Availability: Europe, Middle East & AfricaCAS Number: 85507-79-5EC Number: 287-401-6Information provided by ExxonMobil |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Natural resin extruded under proper conditions with black masterbatch DFNF-0092 (6.5%); ASTM D792 |
Dow CONTINUUM™ DGDA-2490 NT Bimodal Polyethylene Resin CONTINUUM™ DGDA-2490 NT is produced using UNIPOL™ II process technology. This product may be utilized for pipe applications where long term hydrostatic strength combined with outstanding resistan.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Natural resin extruded under proper conditions with black masterbatch DFNF-0092 (6.5%); ASTM D792 |
Dow CONTINUUM™ DGDC-2480 NT Bimodal Polyethylene Resin CONTINUUM™ DGDA-2490 NT is produced using UNIPOL™ II process technology. This product may be utilized for pipe applications where long term hydrostatic strength combined with outstanding resistan.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | |
Abatron AboThane 8003-3 Polyurethane Coating AboThane 8003-3 is a clear one-package, moisture-cure polyurethane coating for hardwood, concrete and seamless floors. It was designed for high flexibility, excellent wear and antiskid properties, .. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Part B |
Abatron Ferrobond-L™ Steel-Filled, Structural Adhesive Putty; Liquid Ferrobond-L™ is a fluid pourable Ferrobond-P™. Casting version of Ferrobond-P™. Choose when flowing consistency is needed for pouring. Excellent for tooling. Technical Characteristics: A: 23 lbs.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Part B |
Abatron SS-Bond-P™ Stainless-Steel-Filled, Structural Adhesive Putty; Paste SS-Bond-P™ is a stainless-steel-filled structural adhesive putty. Used where a filler is needed that is as heavy, hard, and wear resistant as iron, but rustproof and more chemical resistant. Common.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM-D792 |
Braskem HC7260LS-L HDPE Injection Molding Polyethylene HC7260LS-L is a high-density polyethylene developed for injection molding. It has high hardness and stiffness and low warpage. This resin also has additives against ultraviolet radiation action. Its.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | AboCure 50-4 |
Abatron AboCast 22-30/AboCure 50-4 Epoxy AboCast 22-30 is a black filled resin with high viscosity and a weight of 12.4 lbs/gallon. AboCure 50-4 is clear, slow converter with a variable ratio, low viscosity, and a weight of 8 lbs/gallon. A.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Part B |
Abatron BronzeWeld-P™ Bronze-Filled, Structural Adhesive Putty; Paste BronzeWeld-P™ is a bronze-filled structural adhesive putty. Ideal for statuary, antiques, boats, transportation equipment, vases, railings, metal furniture, metal trim, frames, and instruments. Use.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM-D792 |
Braskem IE59U3 HDPE Injection Molding Polyethylene Homopolymer IE59U3 is a high-density polyethylene, narrow molecular weight homopolymer produced by the solution process for injection molding applications. It offers high stiffness and impact strength, good pro.. |