Material Notes:
3M™ Adhesive Transfer Tape 1026 is a 300 high strength acrylic adhesive on a 4 mil liner. Adhesive transfer tape in a pre-cut, tape strip on a pad.Features:5.0 mil adhesive transfer tape on a pad. Kraft paper liner. For a wide variety of materialsGood UV resistance. Good chemical resistance. Ideal for high surface energy (HSE) and low surface energy (LSE) materials.Used as a general transfer tape for a variety of high tack, thin applications.General Industrial Applications, Packaging, Graphic AttachmentThis is good for adhering, joining, affixing, bonding, mounting, holding, laminating and attaching. Recouperage packaging applications. Re-sealing lids on beverage cartons or other boxes. Laminating adhesive for foams, photos, fabrics, metal or plastic Information provided by 3M
Physical Properties Metric English Comments
Thickness 102 microns
4.00 mil
Release Liner
127 microns
5.00 mil
Tape Only
Mechanical Properties Metric English Comments
Peel Strength 0.82172 kN/m
4.6875 pli
to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Long term
121 °C
250 °F
Short term
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Carrier None
Adhesive Type #300 adhesive family
Appearance Clear
Liner Tan Kraft Paper
Users viewing this material also viewed the following: