3M 1449 General Purpose Aluminum Foil Tape

Category Metal , Nonferrous Metal , Aluminum Alloy , Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 1449 General Purpose Aluminum Foil Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
1.4 mil backing; thin aluminum foil tape for conformability.Information provided by 3M
Physical Properties Metric English Comments
Thickness 35.6 microns
1.40 mil
Backing; ASTM D3652
66.0 microns
2.60 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.5 MPa
7320 psi
ASTM D3759
Peel Strength 0.40538 kN/m
2.3125 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -32.0 °C
-25.6 °F
Descriptive Properties Value Comments
Adhesive Type Acrylic