3M 5421 Polyethylene Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 5421 Polyethylene Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Polyethylene Tape 5421 has a rubber adhesive which provides an excellent abrasion resistant surface.Information provided by 3M
Physical Properties Metric English Comments
Thickness 88.9 microns
3.50 mil
Liner; ASTM D3752
127 microns
5.00 mil
Backing; ASTM D3752
170 microns
6.70 mil
Total without liner; ASTM D3752
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.9 MPa
4480 psi
ASTM D3759
Elongation at Break 275 %
275 %
ASTM D3759
Peel Strength 0.2849 kN/m
1.625 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 107 °C
225 °F
Minimum Service Temperature, Air -34.0 °C
-29.2 °F
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Translucent