Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 107 °C | 225 °F | |
Parker Chomerics CHO-FLEX 602 Conductive Coating CHO-FLEX™ 602 is a two-component silver-filled polyurethane coating designed for room temperature or oven cure. CHOFLEX™
602 coating can be sprayed on large panels, cured at room temperature and .. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
Saint-Gobain CHR® 2300-10R UHMW Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: UHMW polyolefin film tape provides anti-sticking and abrasion resistance properties for application temperatures ranging from -100°F to 225°F (-73°C to +107°C). Applications.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
Saint-Gobain CHR® 2300-5R UHMW Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: UHMW polyolefin film tape provides anti-sticking and abrasion resistance properties for application temperatures ranging from -100°F to 225°F (-73°C to +107°C). Applications.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
Saint-Gobain CHR® 2302-10R UHMW Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: UHMW polyolefin film tape provides anti-sticking and abrasion resistance properties for application temperatures ranging from -100°F to 225°F (-73°C to +107°C). Applications.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Heat deflection temperature, load unknown; ASTM D648 |
Toyobo PELPRENE™ S2001 Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
Loctite® 312 Acrylic Bonding Adhesive Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. .. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
Loctite® 410 Toughened Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Continuous |
DuPont™ Tedlar® SP TTR5JAM9 Transparent Polyvinyl Fluoride Film Transparent, Medium Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resista.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Continuous |
DuPont™ Tedlar® SP TUA10AH9 Polyvinyl Fluoride Film UV Screening, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistan.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Continuous |
DuPont™ Tedlar® TTR10BG3 Transparent Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M 6035PC 12028 Polyurethane Foam Tape (15 lb./ft3 (239 kg/m3) Series) 3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M 6035PC 12032 Polyurethane Foam Tape (15 lb./ft3 (239 kg/m3) Series) 3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Intermittent Exposure |
3M Bumpon™ SJ5216 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Intermittent Exposure |
3M Bumpon™ SJ5904 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Intermittent Exposure |
3M Bumpon™ SJ6016 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Intermittent Exposure |
3M Bumpon™ SJ6216 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M Scotchcal™ ElectroCut™ 407 Graphic Film Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high at.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Intermittent |
3M SJ6344 Protective Product, Molded Shapes 3M Bumpon Protective Products SJ6344 is a pressure-sensitive adhesive-backed, molded polyurethane product. The Bumpon SJ6344 is called an Easy Slide Series because it incorporates a special abrasion.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M 3302 Specialty Foil Tape Aluminum foil tape. EMI/RFI shielding. Ul 510 Recognized.Information provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M 421 Lead Foil Tape Self-wound plating tapeInformation provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M 5421 Polyethylene Tape 3M™ Polyethylene Tape 5421 has a rubber adhesive which provides an excellent abrasion resistant surface.Information provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M 5423 Polyethylene Tape 3M™ Polyethylene Tape 5422 has a rubber adhesive which provides an excellent abrasion resistant surface.Information provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M 5425 UHMW Polyethylene Tape 3M™ UHMW Polyethylene Tape 5425 is a film coated with a special acrylic adhesive that is resistant to many solvents.Information provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M 6035PC 12026 Polyurethane Foam Tape (15 lb./ft3 (239 kg/m3) Series) 3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M 6035PC 12049 Polyurethane Foam Tape (20 lb./ft3 (320 kg/m3) Series) 3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Intermittent Exposure |
3M Bumpon™ SJ6208 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M Scotchcal™ ElectroCut™ 404 Graphic Film Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high at.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Intermittent |
3M SJ5202 Protective Product, Die Cut Shapes 3M Bumpon Protective Products SJ5201 and SJ5202 are pressure-sensitive, adhesive backed polyurethane products made from SJ5200 Series soft foam rollstock. A hexagon shape is often preferred for vari.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
Loctite® Black Max® 380 Instant Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
Henkel Hysol EA 9394.2 Paste Adhesive System Fast cure adhesive for liquid shim and potting. Handling strength within 6 - 8 hours.Applications: Potting Structural Repair Liquid Shim |