3M 7897 Computer-Imprintable Polyester Label Material

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7897 Computer-Imprintable Polyester Label Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 310 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasion resistance in bar code applications. Adhesive has right balance of performance and price.Excellent adhesion to HSE plastics and metals3M Performance Label offers wide range of products for long term durability and adhesion with automotive chemical resistance and outdoor durability. Some products are UL/CSA compliant materials that can be printed by Flexographic or Screen Print processes, as well as Thermal Transfer, Digital Printing, Inkjet, Laser or Dot Matrix Printing. Available with many facestocks such as Polyester, Polypropylene and Vinyl to Pharmaceutical papers or synthetics. Please refer to individual Product Datapage for specific product details.Think 3M First for Label Materials used in these Key Markets - Automotive, Electronics, Medical Device, Outdoor Power Equipment, Health Care, Security, Government, Personal Care, Recreational Vehicle, Aerospace, Transportation, Packaging, Foam Fabrication and General Industrial.Typical 3M Performance Label Applications include Bar Code Tracking, Track and Trace, Thermal Transfer Labels, Variable Information Printing (VIP), Brand and Instruction Labels, Warning Labels, Durable Decals, Surface Protection and Masking, Over Laminate, UV Protection, Tamper Indicating, Destructable Labels, Void Message, Fraud Reduction, Laminating, Bonding and Digital Window Graphics.Information provided by 3M
Physical Properties Metric English Comments
Thickness 20.3 microns
0.800 mil
Adhesive
58.4 microns
2.30 mil
Facestock
81.3 microns
3.20 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.05478 kN/m
0.3125 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.0877 kN/m
0.500 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.131 kN/m
0.750 pli
LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.175 kN/m
1.00 pli
Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.175 kN/m
1.00 pli
HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.1972 kN/m
1.125 pli
Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.1972 kN/m
1.125 pli
Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.219 kN/m
1.25 pli
LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.219 kN/m
1.25 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.219 kN/m
1.25 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.219 kN/m
1.25 pli
LD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.2410 kN/m
1.375 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.263 kN/m
1.50 pli
HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.263 kN/m
1.50 pli
Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.263 kN/m
1.50 pli
LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.29582 kN/m
1.6875 pli
Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.29582 kN/m
1.6875 pli
HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.3287 kN/m
1.875 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.3287 kN/m
1.875 pli
Polypropylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.351 kN/m
2.00 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.351 kN/m
2.00 pli
Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.351 kN/m
2.00 pli
Glass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.36156 kN/m
2.0625 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.3725 kN/m
2.125 pli
Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.38347 kN/m
2.1875 pli
Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.38347 kN/m
2.1875 pli
Polypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.38347 kN/m
2.1875 pli
HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.40538 kN/m
2.3125 pli
Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.4163 kN/m
2.375 pli
Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.438 kN/m
2.50 pli
Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.44921 kN/m
2.5625 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.44921 kN/m
2.5625 pli
Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.4602 kN/m
2.625 pli
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.47112 kN/m
2.6875 pli
Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.47112 kN/m
2.6875 pli
Polycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.5040 kN/m
2.875 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.5040 kN/m
2.875 pli
Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.51494 kN/m
2.9375 pli
Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.51494 kN/m
2.9375 pli
Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.55877 kN/m
3.1875 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.570 kN/m
3.25 pli
Glass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.570 kN/m
3.25 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.657 kN/m
3.75 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.6793 kN/m
3.875 pli
Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.7231 kN/m
4.125 pli
Glass, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.745 kN/m
4.25 pli
Glass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.745 kN/m
4.25 pli
Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.8108 kN/m
4.625 pli
Stainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type #310 Acrylic
Liner 55# Densified kraft